Garlock 9780 Fluoroelastomer Sheet Rubber Gasketing

Category Polymer , Thermoset , Fluoropolymer, TS , Thermoset Fluoroelastomer
Manufacturer Garlock Rubber Technologies
Trade Name
Port Ningbo port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Garlock 9780 Fluoroelastomer Sheet Rubber Gasketing.pdf
Price EMAIL US    sales@lookpolymers.com
Material Notes:
Proprietary blend of fluoroelastomer.Resistant to severe chemicals and steam.Information provided by Garlock Rubber Technologies
Mechanical Properties Metric English Comments
Hardness, Shore A 60 - 80
60 - 80
ASTM D 2240
Tensile Strength 8.27 MPa
1200 psi
ASTM F152
Elongation at Break >= 175 %
>= 175 %
ASTM D 395
Thermal Properties Metric English Comments
Maximum Service Temperature, Air 204 °C

@Pressure 1.72 MPa
400 °F

@Pressure 250 psi
Minimum Service Temperature, Air -26.1 °C
-15.0 °F
Descriptive Properties Value Comments
Color Black