Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

Gouda Vuurvast AK 70 KP Dense Refractory Brick

Category Ceramic , Oxide , Aluminum Oxide , Silicon Oxide
Manufacturer Gouda Vuurvast
Trade Name
Port Shanghai port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Gouda Vuurvast AK 70 KP Dense Refractory Brick.pdf
Price EMAIL US    sales@lookpolymers.com
Material Notes:
Description: A high quality phosphate bonded andalusite/corundum brick with very good volume stability. Also good slag resistance and thermal shock resistance. Remarks: This data represents average values, obtained from samples that were cut from standard bricks.Information provided by Gouda Vuurvast.
Physical Properties Metric English Comments
Density 2.65 g/cc
0.0957 lb/in³
Apparent
Porosity 16 %
16 %
Apparent
Mechanical Properties Metric English Comments
Compressive Strength 75.0 MPa
10900 psi
Cold Crushing Strength
Thermal Properties Metric English Comments
Thermal Conductivity 1.90 W/m-K

@Temperature 1100 °C
13.2 BTU-in/hr-ft²-°F

@Temperature 2010 °F
2.00 W/m-K

@Temperature 650 °C
13.9 BTU-in/hr-ft²-°F

@Temperature 1200 °F
2.20 W/m-K

@Temperature 100 °C
15.3 BTU-in/hr-ft²-°F

@Temperature 212 °F
Maximum Service Temperature, Air 1700 °C
3090 °F
1730 °C
3150 °F
Deformation under load - t<sub>a</sub>
Component Elements Properties Metric English Comments
Al2O3 70 %
70 %
Fe2O3 0.80 %
0.80 %
SiO2 26 %
26 %
Descriptive Properties Value Comments
Segercone 38
Thermal Shock Resistance 30 cycles
DIN 51068
Users viewing this material also viewed the following: