Material Notes:
Description: Curon 100 C can be applied up to 1000°C, under normal operating conditions and is especially applied in the bottom of electrolytic cells in the aluminum industry.Remarks: These values apply to cast products.Information provided by Gouda Vuurvast.
Physical Properties Metric English Comments
Bulk Density 1.85 - 1.95 g/cc
0.0668 - 0.0704 lb/in³
After drying at 110°C
Particle Size <= 8000 µm
<= 8000 µm
Grain Size
Mechanical Properties Metric English Comments
Compressive Strength 20.0 - 30.0 MPa

@Temperature 1000 °C
2900 - 4350 psi

@Temperature 1830 °F
Cold Crushing Strength
50.0 - 60.0 MPa

@Temperature 100 °C
7250 - 8700 psi

@Temperature 212 °F
Cold Crushing Strength
Thermal Properties Metric English Comments
Thermal Conductivity 0.450 - 0.550 W/m-K

@Temperature 100 °C
3.12 - 3.82 BTU-in/hr-ft²-°F

@Temperature 212 °F
0.490 - 0.590 W/m-K

@Temperature 600 °C
3.40 - 4.09 BTU-in/hr-ft²-°F

@Temperature 1110 °F
0.530 - 0.630 W/m-K

@Temperature 1000 °C
3.68 - 4.37 BTU-in/hr-ft²-°F

@Temperature 1830 °F
Maximum Service Temperature, Air 1000 °C
1830 °F
Shrinkage -0.100 - 0.500 %

@Temperature 1000 °C
-0.100 - 0.500 %

@Temperature 1830 °F
Permanent Linear Change
Component Elements Properties Metric English Comments
Al2O3 25 %
25 %
SiO2 55 %
55 %
Descriptive Properties Value Comments
Material Consumption per 1 m3 1800 kg
Mixing Water 13-17 liters
per 100 kgs dry material