Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

Gouda Vuurvast CURON 150 Dense Refractory Castable

Category Ceramic , Oxide , Aluminum Oxide
Manufacturer Gouda Vuurvast
Trade Name CURON
Port Ningbo port,China
Trade Terms EXW, FOB, CFR, CIF
Payment Terms L/C, T/T, PayPal
Download PDF Gouda Vuurvast CURON 150 Dense Refractory Castable.pdf
Price EMAIL US    sales@lookpolymers.com
Material Notes:
Description: This bauxite based castable has a very good thermal shock resistance and is therefore well suited for burner blocks.Remarks: These values apply to cast products. Also available in gunning variety, marked "GM". Other modifications are available on demand.Information provided by Gouda Vuurvast.
Physical Properties Metric English Comments
Bulk Density 2.50 - 2.60 g/cc
0.0903 - 0.0939 lb/in³
After drying at 110°C
Particle Size <= 7000 µm
<= 7000 µm
Grain Size
Mechanical Properties Metric English Comments
Compressive Strength 35.0 - 45.0 MPa

@Temperature 1400 °C
5080 - 6530 psi

@Temperature 2550 °F
Cold Crushing Strength
50.0 - 60.0 MPa

@Temperature 100 °C
7250 - 8700 psi

@Temperature 212 °F
Cold Crushing Strength
Thermal Properties Metric English Comments
Thermal Conductivity 0.770 - 0.870 W/m-K

@Temperature 100 °C
5.34 - 6.04 BTU-in/hr-ft²-°F

@Temperature 212 °F
0.820 - 0.920 W/m-K

@Temperature 600 °C
5.69 - 6.38 BTU-in/hr-ft²-°F

@Temperature 1110 °F
0.950 - 1.05 W/m-K

@Temperature 1400 °C
6.59 - 7.29 BTU-in/hr-ft²-°F

@Temperature 2550 °F
Maximum Service Temperature, Air 1600 °C
2910 °F
Shrinkage -1.00 - 1.00 %

@Temperature 1400 °C
-1.00 - 1.00 %

@Temperature 2550 °F
Permanent Linear Change
Component Elements Properties Metric English Comments
Al2O3 80 %
80 %
SiO2 9.0 %
9.0 %
Descriptive Properties Value Comments
ASTM Classification E
Material Consumption per 1 m3 2450 kg
Mixing Water 10-12 liters
per 100 kgs dry material