Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

GrafTech GRAFOIL® GHH Standard Internal Combustion Laminate, Metal Reinforced

Category Carbon , Graphite
Manufacturer GrafTech International
Trade Name GRAFOIL®
Port Ningbo port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF GrafTech GRAFOIL® GHH Standard Internal Combustion Laminate, Metal Reinforced.pdf
Price EMAIL US    sales@lookpolymers.com
Material Notes:
GRAFOIL® Grade GHH is a laminate made with GRAFOIL® Grade GTC flexible graphite chemically bonded to both faces of a flat, low-carbon steel core. Its applications include: exhaust sealing, gasoline/diesel head gaskets, EGR valve sealing, and turbo charger gaskets. While maintaining an effective seal, GRAFOIL® material exhibits virtually no creep relaxation. As a result, the need for periodic bolt tightening is greatly reduced. Laminate Construction: GRAFOIL® Grade GTC ? micro-thin, phenolic-based adhesive ? 0.004" thick Low-Carbon Steel Grade 1008 or 1010 ? micro-thin, phenolic-based adhesive ? GRAFOIL® Grade GTC
Physical Properties Metric English Comments
Bulk Density 1.12 g/cc
0.0405 lb/in³
Standard; Graphite
Thickness 610 microns
24.0 mil
Standard; Laminate
860 microns
33.9 mil
Standard; Laminate
1630 microns
64.2 mil
Standard; Laminate
Mechanical Properties Metric English Comments
Compression Set 83 %
83 %
Air Aging (5 hours at 540°C)
74 %

@Pressure 34.5 MPa
74 %

@Pressure 5000 psi
after 5000 psi load
Descriptive Properties Value Comments
Compressibility (%) 36
at 5000 psi load
41
Air Aging (5 hours at 540°C)