H.C. Starck Grade A Molybdenum Disilicide MoSi2

Category Ceramic
Manufacturer H.C. Starck
Trade Name
Port Shanghai port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF H.C. Starck Grade A Molybdenum Disilicide MoSi2.pdf
Price EMAIL US    sales@lookpolymers.com
Material Notes:
Composite ceramicsHeating elementsConstituent of glow plugs for enginesRaw material for MoSi2 sputter target (PVD)
Physical Properties Metric English Comments
Particle Size 5.5 - 7.5 µm
5.5 - 7.5 µm
Average Particle Size/Laser Diffraction D50
Specific Surface Area <= 1.0 m²/g
<= 1.0 m²/g
BET
Component Elements Properties Metric English Comments
Iron, Fe <= 0.010 %
<= 0.010 %
Oxygen, O <= 0.50 %
<= 0.50 %
Silicon, Si 36.3 - 36.9 %
36.3 - 36.9 %