Henkel Hysol EA 9658 Film Adhesive

Category Polymer , Adhesive , Film , Thermoset , Epoxy , Epoxy Adhesive
Manufacturer Henkel
Trade Name Hysol
Port Ningbo port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Henkel Hysol EA 9658 Film Adhesive.pdf
Price EMAIL US    sales@lookpolymers.com
Material Notes:
High temperature and high durability film adhesive designed for high toughness and high temperature performanceApplications: Composite Bonding Metal and Honeycomb Bonding
Physical Properties Metric English Comments
Storage Temperature -18.0 °C
-0.400 °F
Mechanical Properties Metric English Comments
Tensile Strength 7.00 MPa
1020 psi
Flatwise
Adhesive Bond Strength 19.0 MPa

@Temperature 177 °C
2760 psi

@Temperature 351 °F
Lap Shear
27.0 MPa

@Temperature -55.0 °C
3920 psi

@Temperature -67.0 °F
Lap Shear
33.0 MPa

@Temperature 25.0 °C
4790 psi

@Temperature 77.0 °F
Lap Shear
Thermal Properties Metric English Comments
Maximum Service Temperature, Air 177 °C
351 °F
Glass Transition Temp, Tg 150 °C
302 °F
wet
200 °C
392 °F
dry
Processing Properties Metric English Comments
Cure Time 60.0 min

@Temperature 177 °C
1.00 hour

@Temperature 351 °F
Descriptive Properties Value Comments
Honeycomb Climbing Drum Peel, mN/m 50
at 25°C
Out-Time (days) 15
at 25°C