Material Notes:
Hexcel manufactures aramid fabrics for use in aerospace applications as well as marine, tooling and recreational products where high strength, low weight, and impact resistance are essential. Aramids display excellent dimensional stability with a slightly negative coefficient of thermal expansion (-2.4 X 10-6/ºC.) They are resistant to chemicals with the exception of a few strong acids and alkalis.Aramids have excellent stability over a wide range of temperatures for prolonged periods. They show essentially no embrittlement or strength loss at temperatures as low as -320ºF (-196ºC). Aramids do not melt or support combustion but will start to carbonize at approximately 800ºF (427ºC).Information provided by Hexcel
Physical Properties Metric English Comments
Thickness 330 microns
13.0 mil
Fiber Count 2400 dtex
2160 denier
Warp yarn; Kevlar® 49
2400 dtex
2160 denier
Fill yarn; Kevlar® 49
Mechanical Properties Metric English Comments
Tensile Impact 55.5 J/cm
104 ft-lb/in
Warp
55.5 J/cm
104 ft-lb/in
Filling
Thermal Properties Metric English Comments
CTE, linear -2.40 µm/m-°C
-1.33 µin/in-°F
Maximum Service Temperature, Air 427 °C
801 °F
starts to carbonize
Minimum Service Temperature, Air -196 °C
-321 °F
Descriptive Properties Value Comments
Fabric Weight (oz/yd2) 9.4
Dry
Nominal Construction (count/in) 16
Warp
16
Fill
Weave Style 5 Harness Satin