Hexcel® HexForce™ GA160 Carbon Fabric

Category Carbon , Carbon Fiber
Manufacturer Hexcel
Trade Name HexForce™
Port Shanghai port,China
Trade Terms EXW, FOB, CFR, CIF
Payment Terms L/C, T/T, PayPal
Download PDF Hexcel® HexForce™ GA160 Carbon Fabric.pdf
Price EMAIL US    sales@lookpolymers.com
Material Notes:
Hexcel's carbon fibers contain high strength-to-weight and stiffness-to-weight ratios. Carbon fabrics are thermally and electrically conductive and exhibit excellent fatigue resistance. When properly engineered, carbon fabric composites can achieve the strength and stiffness of metals at significant weight savings. Hexcel's carbon fabrics are compatible with various resin systems including epoxy, polyester and vinyl ester resins.Information provided by Hexcel
Mechanical Properties Metric English Comments
Tensile Modulus 228 GPa
33000 ksi
12K Carbon Warp Yarn
Descriptive Properties Value Comments
Fabric Weight (oz/yd2) 15.7
Dry
Nominal Construction (count/in) 16
Warp
4
Fill
Weave Style Plain Heatset