Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

Hexcel® HexForce™ XLS9114 Carbon/Wire Fabric

Category Carbon , Carbon Fiber , Other Engineering Material , Composite Fibers
Manufacturer Hexcel
Trade Name HexForce™
Port Shanghai port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Hexcel® HexForce™ XLS9114 Carbon/Wire Fabric.pdf
Price EMAIL US    sales@lookpolymers.com
Material Notes:
Hexcel features custom fabric design and manufacturing. We tailor our customers' reinforcement fabrics for optimum performance. We are able to combine two or more different fibers (carbon, glass, aramid, ceramics, Thorstrand™), to use different weaving solutions, produce preforms, etc.Information provided by Hexcel
Descriptive Properties Value Comments
Fabric Weight (g/m2) 260
Dry
Nominal Construction (count/in) 11.2
Warp
11.2
Fill
Type of Yarn Fill Yarn: 0.004" dia Ni Plated Cu
Fill Yarn: Soficar T800HB 6K
Warp Yarn: 0.004" dia Ni Plated Cu
Warp Yarn: Soficar T800HB 6K
Weave Style Double Plain