Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

Hexcel® HexPly® F515 Epoxy Resin

Category Polymer , Thermoset , Epoxy , Epoxy Cure Resin
Manufacturer Hexcel
Trade Name HexPly®
Port Shanghai port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Hexcel® HexPly® F515 Epoxy Resin.pdf
Price EMAIL US    sales@lookpolymers.com
Material Notes:
HexPly® F515 is an advanced, industrial grade, modified epoxy formulation designed for either vacuum bag or autoclave curing to offer very high laminate strengths, coupled with increased fracture toughness. HexPly® F515 has a 250°F (121°C) cure.Information provided by HexCel
Physical Properties Metric English Comments
Specific Gravity 1.20 g/cc
1.20 g/cc
Mechanical Properties Metric English Comments
Tensile Strength, Yield 41.0 MPa
5950 psi
Elongation at Yield >= 1.6 %
>= 1.6 %
Tensile Modulus 3.10 GPa
450 ksi
Thermal Properties Metric English Comments
Glass Transition Temp, Tg 124 °C
255 °F
Dry
Processing Properties Metric English Comments
Gel Time <= 2.00 min

@Temperature 135 °C
<= 2.00 min

@Temperature 275 °F
6