Hexcel® HexPly® M10E Epoxy Resin

Category Polymer , Thermoset , Epoxy , Epoxy Cure Resin
Manufacturer Hexcel
Trade Name HexPly®
Port Shanghai port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Hexcel® HexPly® M10E Epoxy Resin.pdf
Price EMAIL US    sales@lookpolymers.com
Material Notes:
HexPly® M10E is an epoxy resin system preimpregnated into aramid, glass or graphite multiaxial fabrics and unidirectional fibers. M10E prepregs are recommended for the production of low cost, large thick-sectioned industrial structures.Information provided by HexCel
Physical Properties Metric English Comments
Density 1.19 g/cc
0.0430 lb/in³
Mechanical Properties Metric English Comments
Hardness, Barcol 33
33
Thermal Properties Metric English Comments
Glass Transition Temp, Tg 90.0 °C
194 °F
Wet
116 °C
241 °F
Dry