Category Polymer , Film , Thermoplastic , Fluoropolymer , Polychlorotrifluoroethylene (PCTFE); Molded
Manufacturer
Trade Name
Port Ningbo port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Honeywell ACLAR® 11A (4.00 mil) CTFE Homopolymer, Barrier Film  (discontinued **).pdf
Price EMAIL US    sales@lookpolymers.com
Material Notes:
Description: ACLAR® 11A is a CTFE homopolymer, high performance barrier film for industrial and electronics applications.Information provided by Honeywell.
Physical Properties Metric English Comments
Specific Gravity 2.11 g/cc
2.11 g/cc
ASTM D1505
Density 2.13 g/cc
0.0770 lb/in³
Yield Density
Water Vapor Transmission 0.0600 g/m²/day
0.00386 g/100 in²/day
100°F (37.8°C) / 100%RH; ASTM F1249
Thickness 102 microns
4.00 mil
Mechanical Properties Metric English Comments
Film Elongation at Break, MD 150 - 225 %
150 - 225 %
ASTM D882
Film Elongation at Break, TD 175 - 250 %
175 - 250 %
ASTM D882
Secant Modulus, MD 1.207 - 1.551 GPa
175.1 - 225.0 ksi
ASTM D882
Secant Modulus, TD 1.207 - 1.551 GPa
175.1 - 225.0 ksi
ASTM D882
Tear Strength Test 450 - 525
450 - 525
graves tear MD, grams/mil; ASTM D1004
450 - 525
450 - 525
graves tear TD, grams/mil; ASTM D1004
Film Tensile Strength at Break, MD 34.5 - 41.4 MPa
5000 - 6000 psi
ASTM D882
Film Tensile Strength at Break, TD 34.5 - 41.4 MPa
5000 - 6000 psi
ASTM D882
Thermal Properties Metric English Comments
Thermal Conductivity 0.209 W/m-K
1.45 BTU-in/hr-ft²-°F
Melting Point 211 °C
412 °F
crystalline melting point; ASTM D4591
Oxygen Index 100 %
100 %
ASTM D2863
Shrinkage, MD <= 2.0 %
<= 2.0 %
300°F / 149°C - 10 min.; ASTM D1204
Shrinkage, TD <= 2.0 %
<= 2.0 %
300°F / 149°C - 10 min.; ASTM D1204
Optical Properties Metric English Comments
Haze <= 1.0 %
<= 1.0 %
ASTM D1003
Descriptive Properties Value Comments
Flammability non flammable