Huntsman Araldite GY 507 Bisphenol A Epoxy Liquid Resin

Category Polymer , Thermoset , Epoxy , Epoxy Encapsulant, Unreinforced
Manufacturer Huntsman, former Ciba Specialty Chemicals
Trade Name Araldite
Port Ningbo port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Huntsman Araldite GY 507 Bisphenol A Epoxy Liquid Resin.pdf
Price EMAIL US    sales@lookpolymers.com
Material Notes:
Weight per Epoxide (EEW, g/eq) 180 to 192. Max color is 3.Comments/Applications: GY 6010 modified with DY 023 (CGE) - a monofunctional reactive diluent. General purpose, modified resin. Very low tendency to crystallize.Data provided by Ciba Specialty Chemicals.Ciba Specialty Chemicals has been acquired by Huntsman.
Physical Properties Metric English Comments
Viscosity 500 - 700 cP
500 - 700 cP