Material Notes:
Weight per Epoxide (EEW, g/eq) 109 to 117. Color: BrownComments/Applications: Lowest viscosity, tetra-functional epoxy with the same chemistry as MY 720. Used for high performance composites, adhesives, laminates and high energy radiation resistant components.Data provided by Ciba Specialty Chemicals.Ciba Specialty Chemicals has been acquired by Huntsman.
Physical Properties Metric English Comments
Viscosity 3600 - 5000 cP
3600 - 5000 cP