Hyosung Topilene HJ340 PP

Category Polymer , Thermoplastic , Polypropylene (PP) , Polypropylene, Impact Modified; Molded/Extruded
Manufacturer Hyosung Co.
Trade Name Topilene
Port Ningbo port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Hyosung Topilene HJ340 PP.pdf
Price EMAIL US    sales@lookpolymers.com
Material Notes:
HJ340 Impact CopolymerApplications:Corrugated sheetThick board (tank, etc…)Characteristics:High impactHigh stiffnessLow warpageInformation provided by Hyosung Corporation
Physical Properties Metric English Comments
Melt Flow 1.2 g/10 min
1.2 g/10 min
ASTM D1238
Mechanical Properties Metric English Comments
Hardness, Rockwell R 80
80
ASTM D785
Tensile Strength, Yield 31.4 MPa
4550 psi
ASTM D638
Flexural Modulus 1.47 GPa
213 ksi
ASTM D790
Izod Impact, Unnotched 1.08 J/cm
2.02 ft-lb/in
ASTM D256