Material Notes:
Vinylester compounds in a range of strengths with superior corrosion resistance.Data provided by the manufacturer.
Physical Properties Metric English Comments
Density 1.80 g/cc
0.0650 lb/in³
Water Absorption 0.070 %
0.070 %
in 24 hours; ASTM D570
Linear Mold Shrinkage 0.0020 cm/cm
0.0020 in/in
ASTM D955
Mechanical Properties Metric English Comments
Hardness, Barcol 30 - 40
30 - 40
ASTM D2583
Tensile Strength, Ultimate 69.0 MPa
10000 psi
ASTM D638
Flexural Strength 152 MPa
22000 psi
ASTM D790
Flexural Modulus 13.0 GPa
1890 ksi
ASTM D790
Compressive Strength 186 MPa
27000 psi
ASTM D695
Izod Impact, Notched 6.30 J/cm
11.8 ft-lb/in
ASTM D256
Thermal Properties Metric English Comments
Flammability, UL94 HB

@Thickness 3.20 mm
HB

@Thickness 0.126 in