| Category | Polymer , Thermoplastic , Vinyl (PVC) | 
| Manufacturer | Karina Indústria e Comércio de Plásticos | 
| Trade Name | |
| Port | Shanghai port,China | 
| Trade Terms | FOB, CFR, CIF | 
| Payment Terms | L/C, T/T, Western Union | 
| Download PDF | Karina E 839-10/158-CR White PVC Compound.pdf  | 
          
| Price | EMAIL US sales@lookpolymers.com | 
| Physical Properties | Metric | English | Comments | 
|---|---|---|---|
| Specific Gravity | 1.39 - 1.45 g/cc | 1.39 - 1.45 g/cc | ASTM D 792 | 
| ASTM Color | -1.21 - 0.39 | -1.21 - 0.39 | Color A, ME 12 | 
| -0.060 - 1.54 | -0.060 - 1.54 | Color B, ME 12 | |
| 91.91 - 93.51 | 91.91 - 93.51 | Color L, ME 12 | 
| Mechanical Properties | Metric | English | Comments | 
|---|---|---|---|
| Hardness, Shore D |           78 - 82                     @Time 15.0 sec  | 
                  78 - 82                     @Time 0.00417 hour  | 
        ASTM D 2240 | 
| Tensile Strength | >= 34.3 MPa | >= 4980 psi | ASTM D 638 | 
| Elongation at Break | >= 5.0 % | >= 5.0 % | ASTM D 638 | 
| Descriptive Properties | Value | Comments | 
|---|---|---|
| Application | Fittings |