Karina E818-18/99-CRM Gray PVC Compound

Category Polymer , Thermoplastic , Vinyl (PVC)
Manufacturer Karina Indústria e Comércio de Plásticos
Trade Name
Port Shanghai port,China
Trade Terms EXW, FOB, CFR, CIF
Payment Terms L/C, T/T, PayPal
Download PDF Karina E818-18/99-CRM Gray PVC Compound.pdf
Price EMAIL US    sales@lookpolymers.com
Material Notes:
Information provided by Karina Indústria e Comércio de Plásticos Ltda.
Physical Properties Metric English Comments
Specific Gravity 1.33 - 1.39 g/cc
1.33 - 1.39 g/cc
ASTM D 792
ASTM Color -2.93 - -1.33
-2.93 - -1.33
Color B, ME 12
-1.84 - -0.240
-1.84 - -0.240
Color A, ME 12
43.43 - 45.03
43.43 - 45.03
Color L, ME 12
Mechanical Properties Metric English Comments
Hardness, Shore D 78 - 82

@Time 15.0 sec
78 - 82

@Time 0.00417 hour
ASTM D 2240
Tensile Strength >= 34.3 MPa
>= 4980 psi
ASTM D 638
Thermal Properties Metric English Comments
Vicat Softening Point >= 72.0 °C
>= 162 °F
ASTM D 1525
Descriptive Properties Value Comments
Application Fittings