| Category | Polymer , Thermoplastic , Polycarbonate (PC) |
| Manufacturer | Kazanorgsintez |
| Trade Name | |
| Port | Shanghai port,China |
| Trade Terms | EXW, FOB, CFR, CIF |
| Payment Terms | L/C, T/T, PayPal |
| Download PDF | Kazanorgsintez PC-010 Polycarbonate.pdf |
| Price | EMAIL US sales@lookpolymers.com |
| Physical Properties | Metric | English | Comments |
|---|---|---|---|
| Melt Flow | 8.5 - 11.5 g/10 min @Load 1.20 kg, Temperature 300 °C |
8.5 - 11.5 g/10 min @Load 2.65 lb, Temperature 572 °F |
| Mechanical Properties | Metric | English | Comments |
|---|---|---|---|
| Tensile Strength, Yield | >= 55.0 MPa | >= 7980 psi | 2nd Grade |
| >= 58.0 MPa | >= 8410 psi | 1st Grade | |
| >= 60.0 MPa | >= 8700 psi | Superior Quality | |
| Elongation at Break | >= 80 % | >= 80 % | 2nd Grade |
| >= 100 % | >= 100 % | Superior Quality, 1st Grade | |
| Flexural Modulus | 2.00 GPa | 290 ksi | 2nd Grade |
| 2.25 GPa | 326 ksi | Superior Grade, 1st Grade | |
| Transverse Strength | >= 70.0 MPa | >= 10200 psi | at max sample load |
| >= 80.0 MPa | >= 11600 psi | at max sample load | |
| Compressive Yield Strength | >= 70.0 MPa | >= 10200 psi | 1st Grade, 2nd Grade |
| >= 76.0 MPa | >= 11000 psi | Superior Quality | |
| Izod Impact, Unnotched (ISO) | 66.0 kJ/m² | 31.4 ft-lb/in² |
| Thermal Properties | Metric | English | Comments |
|---|---|---|---|
| Vicat Softening Point | >= 147 °C | >= 297 °F |
| Optical Properties | Metric | English | Comments |
|---|---|---|---|
| Yellow Index | 1.6 - 2.2 % | 1.6 - 2.2 % | Superior Grade |
| 1.0 - 3.5 % | 1.0 - 3.5 % | 1st Grade | |
| Transmission, Visible | 85 % | 85 % | 2nd Grade |
| 89 % | 89 % | Superior Quality, 1st Grade | |
| >= 90 % | >= 90 % | Superior Grade, 1st Grade |
| Electrical Properties | Metric | English | Comments |
|---|---|---|---|
| Dielectric Constant | <= 3.1 @Frequency 1000 Hz |
<= 3.1 @Frequency 1000 Hz |
Superior Quality |
| Dielectric Strength | >= 20.0 kV/mm | >= 508 kV/in | Superior Quality |
| Dissipation Factor | <= 0.0090 @Frequency 1000 Hz |
<= 0.0090 @Frequency 1000 Hz |
Superior Quality |
| Descriptive Properties | Value | Comments |
|---|---|---|
| Amount of impurities [pcs] | 10 | 1st Grade |
| 5 | Superior Quality | |
| Turbidity | 0.8 | Superior Grade, 1st Grade |
| 1 | 2nd Grade |