Material Notes:
Description: Kraton D1153 A is a clear, linear block copolymer based on styrene and butadiene with bound styrene of 29.5% mass. It is supplied from Europe in the physical form(s) identified below in the grade nomenclature: Kraton D1153 AS - supplied as porous pellets dusted with amorphous silicaKraton D1153 AT - supplied as porous pellets dusted with talc Region: Asia Pacific, Europe, Japan, North America, and South America Uses: Kraton D1153 A is used as a modifier of bitumen or thermoplastics and in compound formulations. It may also find use as an ingredient in formulating adhesives, sealants and coatings.Applications: Adhesives, Sealant and Coatings; Bitumen Modification; Compounding and Personal Hygiene; Footwear; Impact Modification; Medical; Packaging and Polymod; Personal Care; and Roads and RoofingInformation provided by Kraton®
Physical Properties Metric English Comments
Specific Gravity 0.940 g/cc
0.940 g/cc
ISO 2781
Bulk Density 0.400 g/cc
0.0145 lb/in³
ASTM D 1895 method B
Volatiles <= 0.30 %
<= 0.30 %
KM 04
Viscosity 1400 - 1900 cP
1400 - 1900 cP
25% Toluene Solution at 25°C; KM 06
Molecular Weight 123000 g/mol
123000 g/mol
Apparent, Triblock; BMS 0490
Melt Flow 3.0 g/10 min

@Load 5.00 kg,
Temperature 200 °C
3.0 g/10 min

@Load 11.0 lb,
Temperature 392 °F
ISO 1133
Ash 0.10 - 0.40 %
0.10 - 0.40 %
AS, AT; ISO 247
Mechanical Properties Metric English Comments
Hardness, Shore A 70

@Time 15.0 sec
70

@Time 0.00417 hour
Measured on compression molded slabs; ASTM D2240
Tensile Strength 28.0 MPa
4060 psi
measured on films cast from a solution in toluene; ISO 37
Elongation at Break 800 %
800 %
Measured on films cast from a solution in toluene; ISO 37
300% Modulus 0.00290 GPa
0.421 ksi
Measured on films cast from a solution in toluene; ISO 37
Descriptive Properties Value Comments
Content Antioxidant
>0.1%, KM 08
Polystyrene
28.5-30.5%, KM 03
Total Extractables
<1.0%, KM 05
Triblock Content 95 percent
BMS 0490