Description: Kraton D1155 B is a clear, linear block copolymer based on styrene and butadiene with bound styrene of 40% mass. It is supplied from South America as indicated in the grade nomenclature: Kraton D1155 BO - supplied as a dusted, porous pelletRegion: Asia Pacific, Europe, Japan, North America, and South America Uses: Kraton D1155 B is used in the modification of polymers and in compounds for technical and footwear applications. It is also used in formulating adhesives, sealants and coatings and as a modifier for bitumen.Applications: Compounding and Personal HygieneInformation provided by Kraton®
Physical Properties Metric English Comments
Specific Gravity 0.940 g/cc
0.940 g/cc
ISO 2781
Bulk Density 0.400 g/cc
0.0145 lb/in³
ASTM D 1895 method B
Volatiles <= 0.50 %
<= 0.50 %
KM 04
Melt Flow 1.8 - 5.0 g/10 min

@Load 2.16 kg,
Temperature 190 °C
1.8 - 5.0 g/10 min

@Load 4.76 lb,
Temperature 374 °F
ISO 1133
Mechanical Properties Metric English Comments
Hardness, Shore A 70
70
Measured on films cast from a solution in toluene; ISO 868
Tensile Strength 33.0 MPa
4790 psi
ISO 37
Elongation at Break 880 %
880 %
ISO 37
300% Modulus 0.00290 GPa
0.421 ksi
ISO 37
Descriptive Properties Value Comments
Content Antioxidant
>0.2%, KM 08
Dust
0.05-0.2%
Polystyrene
37-43%, KM 03
Total Extractables
<1.0%, KM 05