Kraton® FG1901 G (SEBS) Linear Block Copolymer

Category Polymer , Thermoplastic , Elastomer, TPE
Manufacturer Kraton
Trade Name
Port Shanghai port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Kraton® FG1901 G (SEBS) Linear Block Copolymer.pdf
Price EMAIL US    sales@lookpolymers.com
Material Notes:
Description: Kraton FG1901 G is a clear, linear triblock copolymer based on styrene and ethylene/butylene with a polystyrene content of 30%. It is supplied from North America in the physical form identified: FG1901 GT - supplied as a dusted pelletRegion: Asia Pacific, Europe, Japan, North America, and South America Uses: Kraton FG1901 G is used as a modifier of bitumen and polymers. It is also suitable as an ingredient in formulating compounds for footwear applications and may be used in formulating adhesives, sealants, and coatings.Applications: Adhesives, Sealant and Coatings; Compounding and Personal Hygiene; and Impact Modification
Physical Properties Metric English Comments
Specific Gravity 0.910 g/cc
0.910 g/cc
ASTM D792
Brookfield Viscosity 5000 cP

@Temperature 25.0 °C
5000 cP

@Temperature 77.0 °F
25% Toluene solution; BAM 922
Melt Flow 14 - 28 g/10 min

@Load 5.00 kg,
Temperature 230 °C
14 - 28 g/10 min

@Load 11.0 lb,
Temperature 446 °F
ASTM D1238
Mechanical Properties Metric English Comments
Hardness, Shore A 71
71
Typical values on polymer compression molded at 300°F; ASTM D2240
Tensile Strength, Ultimate 34.47 MPa
4999 psi
Typical properties based on film cast from toluene solution.; ASTM D412
Elongation at Break 500 %
500 %
Typical properties based on film cast from toluene solution.; ASTM D412
Descriptive Properties Value Comments
Content Maleic anhydride, Bound
1.4-2.0%, KM 1026
Water
<500 ppmw, at time of packaging
Styrene/Rubber Ratio 30/70