Kuraray HYBRAR® CF1 Mono Layer Cast Film

Category Polymer , Film , Thermoplastic , Elastomer, TPE , Thermoplastic Elastomer, Melt-Processible Rubber
Manufacturer Kuraray Company
Trade Name HYBRAR®
Port Ningbo port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Kuraray HYBRAR® CF1 Mono Layer Cast Film.pdf
Price EMAIL US    sales@lookpolymers.com
Material Notes:
Description: HYBRAR® is another in the series of new high performance thermoplastic rubbers developed by KURARAY using their unique isoprene technology. HYBRAR® is a special thermoplastic rubber which exhibits high vibration damping properties at room temperatures. Both hydrogenated and non-hydrogenated grades of HYBRAR® are available. In addition to the superior vibration damping properties, hydrogenated grades also exhibit excellent miscibility with polypropylene, and may be used to produce blends with excellent transparency, flexibility and mechanical properties.Information provided by The Kuraray Group.
Mechanical Properties Metric English Comments
Film Elongation at Break, MD 1090 %
1090 %
Film Elongation at Break, TD 1130 %
1130 %
Tensile Modulus 0.233 GPa
33.8 ksi
TD
0.235 GPa
34.1 ksi
MD
Film Tensile Strength at Break, MD 38.2 MPa
5540 psi
Film Tensile Strength at Break, TD 35.3 MPa
5120 psi
Optical Properties Metric English Comments
Haze 3.9 %
3.9 %