Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

LG Chemical B160 EPS, Non-Flame Retardant

Category Polymer , Thermoplastic , Polystyrene (PS) , Expanded Polystyrene (EPS)
Manufacturer LG Chemical
Trade Name
Port Shanghai port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF LG Chemical B160 EPS, Non-Flame Retardant.pdf
Price EMAIL US    sales@lookpolymers.com
Material Notes:
Feature: Expendable Polystyrene, Non-Flame RetardantApplication: Package, Fruit/Fish Box, Floats, Pad, Ice BoxCAS No. 9003-53-6 and 109-66-0Information provided by LG Chemical
Physical Properties Metric English Comments
Water Absorption 0.32 %
0.32 %
[g/100cm<sup>2</sup>], 30g/L; KS M 3808
0.35 %
0.35 %
[g/100cm<sup>2</sup>], 25g/L; KS M 3808
0.40 %
0.40 %
[g/100cm<sup>2</sup>], 20g/L; KS M 3808
0.44 %
0.44 %
[g/100cm<sup>2</sup>], 15g/L; KS M 3808
Mechanical Properties Metric English Comments
Flexural Yield Strength 0.181 MPa
26.3 psi
15g/L; KS M 3808
0.275 MPa
39.8 psi
20g/L; KS M 3808
0.363 MPa
52.6 psi
25g/L; KS M 3808
0.392 MPa
56.9 psi
30g/L; KS M 3808
Impact 0.91
0.91
[kg/cm<sup>2<sup>], 15g/L; KS M 3808
1.32
1.32
[kg/cm<sup>2<sup>], 20g/L; KS M 3808
1.75
1.75
[kg/cm<sup>2<sup>], 25g/L; KS M 3808
2.3
2.3
[kg/cm<sup>2<sup>], 30g/L; KS M 3808
Thermal Properties Metric English Comments
Thermal Conductivity 0.0337 W/m-K
0.234 BTU-in/hr-ft²-°F
30g/L; KS M 3808
0.0360 W/m-K
0.250 BTU-in/hr-ft²-°F
25g/L; KS M 3808
0.0372 W/m-K
0.258 BTU-in/hr-ft²-°F
20g/L; KS M 3808
0.0407 W/m-K
0.282 BTU-in/hr-ft²-°F
15g/L; KS M 3808