Lubriplate 1551 Lithium Complex Multi-Purpose Grease

Category Fluid , Lubricant , Lithium Gellant
Manufacturer Lubriplate Lubricants
Trade Name
Port Ningbo port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Lubriplate 1551 Lithium Complex Multi-Purpose Grease.pdf
Price EMAIL US    sales@lookpolymers.com
Material Notes:
These multi-purpose lithium complex lubricants can withstand higher temperatures than traditional lithium greases. They provide high film strength, excellent shear stability, long lubricant life, and exceptional anti-wear properties. Available in four NLGI densities for a variety of applications. No 1552 is NLGI GC-LB certified. Applications: Ind./const./mining equip.1500 Series Greases are available in Pails, 1/4 Drums & Drums. No. 1551 & No. 1552 are also available in Cartridges. Information provided by Lubriplate
Physical Properties Metric English Comments
Saybolt Viscosity at 100°F 1100 SUS
1100 SUS
Kinematic Viscosity at 40°C (104°F) 200 cSt
200 cSt
Mechanical Properties Metric English Comments
Penetration P(0), 1/10 mm 310
310
Unknown Amount of Work
Penetration P(60), 1/10 mm 340
340
Unknown Amount of Work
Thermal Properties Metric English Comments
Minimum Service Temperature, Air -20.6 °C
-5.00 °F
Approx. Cold test
Dropping Point 243 °C
470 °F
ASTM Test
Descriptive Properties Value Comments
Antiwear (AW)/ Extreme Pressure (EP) AW/EP
NLGI Grade 1
Rust/Oxidative Additives YES
Water Resistant YES