Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

Lubriplate 630-AAA Lithium Based Multi-Purpose Grease

Category Fluid , Lubricant , Lithium Gellant
Manufacturer Lubriplate Lubricants
Trade Name
Port Shanghai port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Lubriplate 630-AAA Lithium Based Multi-Purpose Grease.pdf
Price EMAIL US    sales@lookpolymers.com
Material Notes:
These popular lithium type greases are excellent for a wide range of lubrication demands thus reducing the need to carry large grease inventories. They show exceptional resistance to water, steam, and other adverse conditions. Available in 4 NLGI densities for a variety of applications. Applications: Centralized greasing systems.630 Series Greases are available in Cartridges, Tubes, Cans, Pails, 1/4 Drums & Drums.Information provided by Lubriplate
Physical Properties Metric English Comments
Saybolt Viscosity at 100°F 800 SUS
800 SUS
Kinematic Viscosity at 40°C (104°F) 151 cSt
151 cSt
Mechanical Properties Metric English Comments
Penetration P(0), 1/10 mm 355
355
Unknown Amount of Work
Penetration P(60), 1/10 mm 385
385
Unknown Amount of Work
Thermal Properties Metric English Comments
Minimum Service Temperature, Air -23.3 °C
-10.0 °F
Approx. Cold test
Dropping Point 182 °C
360 °F
ASTM Test
Descriptive Properties Value Comments
Antiwear (AW)/ Extreme Pressure (EP) AW/EP
NLGI Grade 0
Rust/Oxidative Additives YES
Water Resistant YES