Lubrizol Advanced Materials Pearlstick® 45-90/06 Polycaprolactone based TPU

Category Polymer , Thermoplastic , Polyurethane, TP
Manufacturer Lubrizol Advanced Materials Manufacturing S. S.L. (Former Merquinsa)
Trade Name Pearlstick®
Port Shanghai port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Lubrizol Advanced Materials Pearlstick® 45-90/06 Polycaprolactone based TPU.pdf
Price EMAIL US    sales@lookpolymers.com
Material Notes:
Pearlstick 45-90/06 is an elastic, linear, aromatic polyurethane, supplied in form of white spherical granules with a small amount of anti-adherent in the formulation. It has a low crystallization rate and a low thermoplasticity level. Solubility: Pearlstick 45-90/06 is soluble in Acetone, Methyl Ethyl Ketone (MEK), Cyclohexanone, Dimethyl Formamide, and Tetrahydrofurane (THF). The solvents and diluents should be water-free (max. 0.1 %), so as to avoid subsequent side reactions during crosslinking with isocyanate. It should be dissolved in closed tanks, and the use of a variable speed agitator is advisable. The final viscosity fies can vary, depending on the stirring process and on the solvent/diluents ratios Applications: Pearlstick 45-90/06 is used for the production of adhesives for different kinds of materials such as leather, textiles, rubber and a variety of plastics (plasticized PVC, PU elastomers, etc.). Pearlstick 45-90/06 enables the production of adhesives with a very long open-time, which can be used as one- or twocomponent adhesives. The addition of a polyfunctional isocyanate to improves the heat-resistance and the strength of the joints. The addition of Pearlstick 45-90/06 to other different types of Pearlstick increases their open-times.Information provided by Merquinsa
Physical Properties Metric English Comments
Density 1.19 g/cc
0.0430 lb/in³
ISO 2781
Brookfield Viscosity 450 - 750 cP
450 - 750 cP
Brookfield RVF sp 3, 20 rpm, Solution 15% MEK (MQSA Nº 55 A); MQSA 40A
Processing Properties Metric English Comments
Processing Temperature 40.0 °C
104 °F
Min. Activation Temp; EN 12961
Descriptive Properties Value Comments
Crystallization Rate (MQSA n° 12 A) LOW
Hydrolysis Resistance Good
MQSA 34B
Hydroxyl Number 0.1%
MQSA 47A
Solubility - Acetone / Ethyl Acetate 70:30
Solubility - Acetone / Toluene 50:50
Solubility - MEK / Toluene 80:20
Solubility - MEK/ Ethyl Acetate 80:20
Thermoplasticity Range (MQSA n° 58) LOW
Users viewing this material also viewed the following:
Copyright © lookpolymers.com All Rights Reserved