Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

Lubrizol ESTANE® 58244 Ether Based Thermoplastic Polyurethane (European Grade)

Category Polymer , Thermoplastic , Elastomer, TPE , Polyurethane, TP , Thermoplastic Polyurethane, Elastomer, Ether Grade
Manufacturer Lubrizol (former Noveon)
Trade Name ESTANE®
Port Shanghai port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Lubrizol ESTANE® 58244 Ether Based Thermoplastic Polyurethane (European Grade).pdf
Price EMAIL US    sales@lookpolymers.com
Material Notes:
Description: Estane® thermoplastic polyurethanes (TPUs) include elastomeric materials that bridge the gap between flexible rubber and rigid plastics. These materials offer toughness and durability in a flexible thermoplastic elastomer system that is easy to process in a wide range of equipment. The Estane® TPU portfolio of products offers high performance polyester - and polyether - based resins and compounds in a broad range of hardnesses to meet a variety of application needs.Benefits of Estane® TPU: Outstanding Abrasion and Wear ResistanceExcellent Low Temperature FlexibilitySuperior Toughness and DurabilityEase of Processing and Manufacturing FlexibilityColorability and Paintability with no adhesion promoterApplications: Film & SheetFabric coating & melt coatingWire & CableHose, Tube & ProfileCustom moldingCustom compoundingAutomotive interior/chassis and exterior painted trimSpecific Notes for this Material: Halogen-free flame retardant Information provided by Noveon, Inc.
Physical Properties Metric English Comments
Specific Gravity 1.19 g/cc
1.19 g/cc
DIN 53479
Mechanical Properties Metric English Comments
Hardness, Shore A 92
92
DIN 53505
Hardness, Shore D 39
39
DIN 53505
Tensile Strength, Ultimate 20.0 MPa
2900 psi
DIN 53504
Elongation at Break 620 %
620 %
DIN 53504
50% Modulus 0.00680 GPa
0.986 ksi
DIN 53504
100% Modulus 0.00780 GPa
1.13 ksi
DIN 53504
300% Modulus 0.00820 GPa
1.19 ksi
DIN 53504
Tear Strength 56.0 kN/m
320 pli
DIN 53515
Abrasion 140
140
mm<sup>3</sup>; DIN 53516