Material Notes:
GUARD DOGâ„¢ UV119 is effective in polypropylene, polyethylene, alpha-olefin copolymers and blends with EPR, ERR, PE, EVA, EAA, EVOH and filled PP.Typical Properties:Appearance - White to light yellow granulesOdor - noneColor of solution@ 425 nm (10% w/v Toluene): 90.0% min
Physical Properties Metric English Comments
Volatiles <= 1.0 %
<= 1.0 %
Solubility in Water >= 0.010 %
>= 0.010 %
Molecular Weight 2285.61 g/mol
2285.61 g/mol
Ash <= 0.10 %
<= 0.10 %
Thermal Properties Metric English Comments
Melting Point 115 - 150 °C
239 - 302 °F
Optical Properties Metric English Comments
UV Transmittance >= 93 %

@Thickness 0.450 mm
>= 93 %

@Thickness 0.0177 in
>= 95 %

@Thickness 0.500 mm
>= 95 %

@Thickness 0.0197 in
Descriptive Properties Value Comments
CAS Number 106990-43-6
Molecular Formula C132H250N32
Name 1,3,5-triazine-2,4,6-triamine,N,N'''-[1,2-ethane-diyl-bis-[[[4,6-bis- [butyl(1,2,2,6,6-pentamethyl-4-piperidinyl)amino]-1,3,5-triazine- 2-yl]imino]-3,1-propanediyl]]-bis[N',N''-bis(1,2,2,6,6-pentamethyl-4-piperidinyl)]