Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

M Chemical GUARD DOGâ„¢ UVP Benzotriazole UV Absorber

Category Other Engineering Material , Additive/Filler for Polymer
Manufacturer M Chemical Company, Inc.
Trade Name GUARD DOG™
Port Shanghai port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF M Chemical GUARD DOGâ„¢ UVP Benzotriazole UV Absorber.pdf
Price EMAIL US    sales@lookpolymers.com
Material Notes:
GUARD DOG™ UVP light stabilizer is a derivative of Benzotriazole that has exceptionally strong and broad-range UV absorption properties (UV A 315 -400 nm and UV B 290 - 314 nm) throughout the UV spectrum. It is a highly efficient UV absorber and is recommended for thermoset plastics and coatings that function as ultraviolet screens for photosensitive substrates.Applications: Extremely effective in Styrenic polymers, PVC, polycarbonate, ABS, unsaturated polyesters, PU, acrylic polymers, natural rubber, synthetic rubber, paints, synthetic fiber, cellulose resin and adhesives.Performance Benefits:Guard Dog™ UVP performs synergistically when used in combination with Hindered Amine Light Stabilizers (HALS)Very high degree of photostability and resistant to oxidizing and reducing agentsHigh heat resistance (5% wt. loss @ 190°C) without significant degradation or volatility at proper extrusion temperature. Does not discolor during light or heat aging.Excellent compatibility with polymers and is odorless. Does not impart smell to the polymer.Typical Properties:Free flowing pale yellowish powderSolubility (g/100g @ 25°C): Acetone 3, Benzene 7, Ethyl Acetate 3, Chloroform 13,Toluene 6Max, nm: 344
Physical Properties Metric English Comments
Specific Gravity 1.38 g/cc

@Temperature 20.0 °C
1.38 g/cc

@Temperature 68.0 °F
Molecular Weight 225.25 g/mol
225.25 g/mol
Thermal Properties Metric English Comments
Melting Point 128 - 132 °C
262 - 270 °F
Descriptive Properties Value Comments
CAS Number 2440-22-4
Molecular Formula C13H11N3O
Name 2-(2'-Hydroxy--5'-methyl-phenyl) benzotriazole