MV Labs BE1000 BeSO4.4H2O Beryllium sulfate tetrahydrate

Category Ceramic
Manufacturer MV Laboratories
Trade Name
Port Ningbo port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF MV Labs BE1000 BeSO4.4H2O Beryllium sulfate tetrahydrate.pdf
Price EMAIL US    sales@lookpolymers.com
Material Notes:
Information provided by MV Laboratories.
Physical Properties Metric English Comments
Molecular Weight 177.14 g/mol
177.14 g/mol
Descriptive Properties Value Comments
Assay 5% Be
CAS Number 7787-56-6
Form White crystals
Purity 99.995%
Typical Impurities Fe, Si = 2; Cu, Al < 1 ppm