MV Labs EU1000 Eu2(SO4)3·8H2O Europium(III) sulfate octahydrate

Category Ceramic
Manufacturer MV Laboratories
Trade Name
Port Shanghai port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF MV Labs EU1000 Eu2(SO4)3·8H2O Europium(III) sulfate octahydrate.pdf
Price EMAIL US    sales@lookpolymers.com
Material Notes:
Information provided by MV Laboratories.
Physical Properties Metric English Comments
Molecular Weight 736.23 g/mol
736.23 g/mol
Descriptive Properties Value Comments
Assay 42% Eu
CAS Number 10031-55-7
Form White crystals
Purity 99.999%
Typical Impurities Ca, Si = 2; Ce = 1; other Rare Earths < 10 ND