Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

MV Labs PD750 Pd(NH3)2(NO2)2 trans-Diaminedinitropalladium(II)

Category Ceramic
Manufacturer MV Laboratories
Trade Name
Port Shanghai port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF MV Labs PD750 Pd(NH3)2(NO2)2 trans-Diaminedinitropalladium(II).pdf
Price EMAIL US    sales@lookpolymers.com
Material Notes:
Information provided by MV Laboratories.
Physical Properties Metric English Comments
Molecular Weight 232.47 g/mol
232.47 g/mol
Descriptive Properties Value Comments
Assay 46% Pd
CAS Number 14852-83-6
Form White crystals
Purity 99.99%
Typical Impurities Na = 10; Ca = 2; Cu, Zn, Ag, Fe, Mg, Na, Pt < 1