| Physical Properties | Metric | English | Comments |
|---|---|---|---|
| Bulk Density | <= 0.750 g/cc | <= 0.0271 lb/in³ | |
| Brightness | >= 92 % | >= 92 % | Whiteness |
| Oil Absorption | <= 22 % | <= 22 % | ml/100g |
| Particle Size | 14 µm | 14 µm | d50 |
| 45 µm | 45 µm | 5% max, wet sieve |
| Component Elements Properties | Metric | English | Comments |
|---|---|---|---|
| Fe2O3 | <= 0.030 % | <= 0.030 % | |
| Na2O | <= 0.30 % | <= 0.30 % | |
| SiO2 | <= 0.030 % | <= 0.030 % |
| Processing Properties | Metric | English | Comments |
|---|---|---|---|
| Moisture Content | <= 0.30 % | <= 0.30 % |
| Descriptive Properties | Value | Comments |
|---|---|---|
| Aluminum Hydroxide (%) | >99.5 | Determined by difference |