Mallard Creek Polymers BarrierPro® 4545 SBR Emulsion

Category Polymer , Thermoset , Rubber or Thermoset Elastomer (TSE) , Styrene Butadiene Rubber
Manufacturer Mallard Creek Polymers
Trade Name BarrierPro®
Port Ningbo port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Mallard Creek Polymers BarrierPro® 4545 SBR Emulsion.pdf
Price EMAIL US    sales@lookpolymers.com
Material Notes:
BARRIER PRO® 4545 is an anionic carboxylated styrene-butadiene copolymer latex. Features: highly stable, good compatibility with fillers and pigments, etc., cured films are tough and pliable, cured films have excellent water resistance, hydrolysis resistant. Storage and handling: Protect from freezing. Ideal storage temperature is 22°C (72°F). Stability at 22°C (72°F) is 180 days when properly stored. Read the BARRIER PRO® 4545 Material Safety Data Sheet before handling, storing, or using this product.APPLICATIONS: BARRIER PRO ® 4545 is a general purpose latex binder of medium to high stiffness. It dries to form a flexible, tough film of high water resistance. BARRIER PRO® 4545 can be compounded with fillers and other additives to form coatings for a variety of applications. Because of its high strength film, it makes an excellent product for blending with other BARRIER PRO® products to strengthen damp proof membranes, specialty paints and sealants.Information provided by Mallard Creek Polymers
Physical Properties Metric English Comments
Solids Content 51 - 53 %
51 - 53 %
pH 8.0 - 8.4
8.0 - 8.4
Brookfield Viscosity 400 - 1200 cP
400 - 1200 cP
#2/20 rpm
Thermal Properties Metric English Comments
Glass Transition Temp, Tg 17.0 °C
62.6 °F