Mallard Creek Polymers ROVENE® 4009 SBR Latex

Category Polymer , Thermoset , Rubber or Thermoset Elastomer (TSE) , Styrene Butadiene Rubber
Manufacturer Mallard Creek Polymers
Trade Name
Port Ningbo port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Mallard Creek Polymers ROVENE® 4009 SBR Latex.pdf
Price EMAIL US    sales@lookpolymers.com
Material Notes:
ROVENE® 4009 is a carboxylated styrene-butadiene emulsion that has a medium hand with above average strength properties. This binder is crosslinkable with external crosslinking agents. ROVENE® 4009 can be compounded into highly water and grease resistant paper and board coatings. It exhibits an excellent balance of water resistance, grease and oil resistance, and low moisture vapor transmission.APPLICATIONS: ROVENE® 4009 is recommended for applications in specialty paper coatings where water, grease and oil resistance is needed.Information provided by Mallard Creek Polymers
Physical Properties Metric English Comments
Solids Content 53 - 55 %
53 - 55 %
Particle Size 0.20 µm
0.20 µm
pH 7.0 - 7.5
7.0 - 7.5
Brookfield Viscosity 100 - 900 cP
100 - 900 cP
#2/20 rpm
Thermal Properties Metric English Comments
Glass Transition Temp, Tg -4.00 °C
24.8 °F
Chemical Properties Metric English Comments
Styrene Content 58 %
58 %
Descriptive Properties Value Comments
Emulsifiers Anionic