| Category | Ceramic , Glass , Glass Ceramic |
| Manufacturer | Mateck GmbH |
| Trade Name | |
| Port | Ningbo port,China |
| Trade Terms | EXW, FOB, CFR, CIF |
| Payment Terms | L/C, T/T, PayPal |
| Download PDF | Mateck Glass (BK7 Schott or analogous).pdf |
| Price | EMAIL US sales@lookpolymers.com |
| Physical Properties | Metric | English | Comments |
|---|---|---|---|
| Density | 2.51 g/cc | 0.0907 lb/in³ |
| Mechanical Properties | Metric | English | Comments |
|---|---|---|---|
| Modulus of Elasticity | 81.0 GPa | 11700 ksi | |
| Poissons Ratio | 0.206 | 0.206 | |
| Shear Modulus | 33.6 GPa | 4870 ksi | Calculated |
| Thermal Properties | Metric | English | Comments |
|---|---|---|---|
| CTE, linear | 7.10 µm/m-°C @Temperature -30.0 - 70.0 °C |
3.94 µin/in-°F @Temperature -22.0 - 158 °F |
|
| Specific Heat Capacity | 0.858 J/g-°C | 0.205 BTU/lb-°F | |
| Thermal Conductivity | 1.114 W/m-K | 7.731 BTU-in/hr-ft²-°F | |
| Melting Point | 559 °C | 1040 °F |
| Optical Properties | Metric | English | Comments |
|---|---|---|---|
| Refractive Index | 1.51872 | 1.51872 | at ne |
| 1.52283 | 1.52283 | at nf' | |
| 1.50731 @Wavelength 1014 nm |
1.50731 @Wavelength 1014 nm |
||
| 1.53626 @Wavelength 365 nm |
1.53626 @Wavelength 365 nm |
||
| IR Transmittance | 75 % @Wavelength 2300 nm |
75 % @Wavelength 2300 nm |
Internal Transmittance |
| 90 % @Wavelength 2000 nm |
90 % @Wavelength 2000 nm |
Internal Transmittance | |
| UV Transmittance | 8.0 % @Wavelength 300 nm |
8.0 % @Wavelength 300 nm |
Internal Transmittance |
| 92 % @Wavelength 350 nm |
92 % @Wavelength 350 nm |
Internal Transmittance |
| Descriptive Properties | Value | Comments |
|---|---|---|
| Thermal Coefficient of Refractive Index | 2.8E-06 | 0.546 microns for ± 20°C |
| Transmission Range (microns) | 0.35 - 2 |