Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

Mearthane Durethaneâ„¢ M DM-710A Foam Polyurethane

Category Polymer , Thermoset , Polyurethane, TS , Thermoset Polyurethane Foam, Unreinforced , Rubber or Thermoset Elastomer (TSE)
Manufacturer Mearthane Products Corporation (MPC)
Trade Name Durethane™ M
Port Shanghai port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Mearthane Durethaneâ„¢ M DM-710A Foam Polyurethane.pdf
Price EMAIL US    sales@lookpolymers.com
Material Notes:
MDI backbone: ether.Shore 00 Hardness: 55Summary: Durethane M is a flexible, microcellular, open cell and closed cell urethane foam. Because it is mechanically mixed, the cell size is uniform. Durethane M is very economical, and has excellent resistance to compression set. It can be formulated to form an integral skin.Applications: The compression set resistance of Durethane M makes it an effective material for applications with repeated compression cycles, such as actuator pads on postal meters and idler belts.Conductivity: All Durethane elastomers can be formulated to be electrically conductive, for applications involving electrostatic dissipation (ESD). Mearthane's proprietary conductivity process does not comprise the material performance specification of the urethane.Information provided by Mearthane Products Corporation.
Physical Properties Metric English Comments
Density 0.320 g/cc
0.0116 lb/in³
ASTM D3574A
Mechanical Properties Metric English Comments
Hardness, Shore A 10
10
ASTM D2240
Tensile Strength, Ultimate 6.90 MPa
1000 psi
ASTM D3574E
Elongation at Break 340 %
340 %
ASTM 3457E
100% Modulus 0.000276 GPa
0.0400 ksi
ASTM D3574E
200% Modulus 0.000620 GPa
0.0899 ksi
ASTM D3574E
Compressive Yield Strength 0.0300 MPa
4.35 psi
at 10% deflection; ASTM D3574C
0.0380 MPa
5.51 psi
at 20% deflection; ASTM D3574C
0.0500 MPa
7.25 psi
at 30% deflection; ASTM D3574C
Resilience 43
43
Bashore Rebound; ASTM 2632D
Tear Strength Test 30
30
lb; Die C; ASTM 3457F