Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

Momentive Performance Materials Addisilâ„¢ 1160 M Industrial Molding Heat Cured Rubber

Category Polymer , Thermoset , Rubber or Thermoset Elastomer (TSE) , Silicone , Silicone Rubber
Manufacturer Momentive Performance Materials (Former GE Silicones)
Trade Name Addisil™
Port Shanghai port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Momentive Performance Materials Addisilâ„¢ 1160 M Industrial Molding Heat Cured Rubber.pdf
Price EMAIL US    sales@lookpolymers.com
Material Notes:
Heat cured rubber is a high consistency product that can be molded, extruded or calendered using conventional rubber processing equipment to meet a wide range of cost, durability and performance standards.Addisil 1160 M is a member of the Addisil Addition Curing Portfolio. It is a platinum (addition/heat) curable, one part ready-to-use compound, all Addisil Industrial Molding grades can be offered as two-part systems. This grade is suitable for molding and intended for industrial applications.
Physical Properties Metric English Comments
Specific Gravity 1.14 g/cc
1.14 g/cc
Mechanical Properties Metric English Comments
Hardness, Shore A 58
58
Tensile Strength 10.5 MPa
1520 psi
Elongation at Break 670 %
670 %
Tear Strength 40.0 kN/m
228 pli
Die B
Optical Properties Metric English Comments
Transmission, Visible 20 %
20 %
translucent; thickness unknown
Compliance Properties Metric English Comments
FDA Yes
Yes
FDA Indirect food contact - Rubber articles intended for repeated use - FDA Reg 21CFR177.2600
Descriptive Properties Value Comments
Appearance Translucent
BfR product is compositionally compliant
Recommendation XV Silicones; post cured (4h/200°C)