Momentive Performance Materials SS4155 Silicone Primer for use with RTV Silicone Adhesive Sealants, Blue

Category Polymer , Adhesive , Thermoset , Silicone , Silicone, RTV, Adhesive/Sealant Grade
Manufacturer Momentive Performance Materials (Former GE Silicones)
Trade Name
Port Ningbo port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Momentive Performance Materials SS4155 Silicone Primer for use with RTV Silicone Adhesive Sealants, Blue.pdf
Price EMAIL US    sales@lookpolymers.com
Material Notes:
SS4004P, SS4044P, SS4120, SS4155, and SS4179 primers are formulated for use with GE Silicones RTV silicone rubber adhesive sealants.  GE Silicones one-component products offer primerless adhesion to many substrates.  Primers are used to help promote adhesion to difficult-to-bond substrates.  For most GE Silicones two-component products, a primer is required when an adhesive bond is needed between the silicone rubber compound and a non-silicone surface (see table below).  All primers are one-component products requiring no mixing and are supplied ready-to-use as easily pourable solvent solutions.SS4155 is a general purpose primer for use with any RTV.Key Performance Properties: One-component - no mixingSimple handling procedures and equipment for easy use and low processing cost.Dry at room temperature and ambient humidity conditionsHelps promote adhesion to many substratesBlue color of SS4155 primer permits easy visual determination of uniform applicationGE Silicones became a part of Momentive Performance Materials in 2006.
Physical Properties Metric English Comments
Specific Gravity 0.820 g/cc
0.820 g/cc
Solids Content 10 %
10 %
Thermal Properties Metric English Comments
Flash Point 37.0 °C
98.6 °F
Pensky-Martin Closed Cup
Processing Properties Metric English Comments
Cure Time 30 min
0.5 hour
Descriptive Properties Value Comments
Color Blue
D.O.T. Label Flammable