| Category | Polymer , Thermoset , Rubber or Thermoset Elastomer (TSE) , Silicone , Silicone Rubber |
| Manufacturer | Momentive Performance Materials (Former GE Silicones) |
| Trade Name | Silplus™ |
| Port | Ningbo port,China |
| Trade Terms | FOB, CFR, CIF |
| Payment Terms | L/C, T/T, Western Union |
| Download PDF | Momentive Performance Materials Silplusâ„¢ 70 MP Heat Cured Rubber.pdf |
| Price | EMAIL US sales@lookpolymers.com |
| Physical Properties | Metric | English | Comments |
|---|---|---|---|
| Specific Gravity | 1.21 g/cc | 1.21 g/cc |
| Mechanical Properties | Metric | English | Comments |
|---|---|---|---|
| Hardness, Shore A | 70 | 70 | |
| Tensile Strength | 11.0 MPa | 1600 psi | |
| Elongation at Break | 420 % | 420 % | |
| Tear Strength | 30.0 kN/m | 171 pli | Die B |
| Optical Properties | Metric | English | Comments |
|---|---|---|---|
| Transmission, Visible | 20 % | 20 % | translucent; thickness unknown |
| Compliance Properties | Metric | English | Comments |
|---|---|---|---|
| FDA | Yes | Yes | FDA Indirect food contact - Rubber articles intended for repeated use - FDA Reg 21CFR177.2600 |
| USP Class VI | Yes | Yes | USP Class VI methods: Intramuscular implantation, intracutaneous injection, & systematic injection |
| Descriptive Properties | Value | Comments |
|---|---|---|
| Appearance | Translucent | |
| BfR | product is compositionally compliant | Recommendation XV Silicones; post cured (4h/200°C) |
| ISO10993 | yes | 7 ISO 10993 tests applicable to "wet" chemicals |
| Water Regulations | compliant | KTW, WRAS, W270 |