Multibase Multi-Flex® RP 6568 TPE Styrene Ethylene Butylene Styrene Block Copolymer

Category Polymer , Thermoplastic
Manufacturer Multibase
Trade Name Multi-Flex®
Port Ningbo port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Multibase Multi-Flex® RP 6568 TPE Styrene Ethylene Butylene Styrene Block Copolymer.pdf
Price EMAIL US    sales@lookpolymers.com
Material Notes:
Features: Chemical Resistance, Good General PurposeOzone Resistant Thermal Stability, Good Forms:PelletsProcessing Method:Injection MoldingBlow MoldingExtrusion Uses: Automotive ApplicationsInformation provided by Multibase
Physical Properties Metric English Comments
Specific Gravity 0.940 g/cc
0.940 g/cc
ASTM 792
Linear Mold Shrinkage 0.020 cm/cm
0.020 in/in
ASTM D955
Melt Flow 2.0 g/10 min

@Load 2.16 kg,
Temperature 230 °C
2.0 g/10 min

@Load 4.76 lb,
Temperature 446 °F
ASTM D1238
Mechanical Properties Metric English Comments
Hardness, Shore A 57
57
10 seconds; ASTM D2240
Tensile Strength, Yield 4.32 MPa
627 psi
ASTM D638
1.38 MPa

@Strain 300 %
200 psi

@Strain 300 %
ASTM D412
Elongation at Break 1400 %
1400 %
ASTM D638
Tear Strength 26.3 kN/m
150 pli
ASTM D624