Material Notes:
The burn rate is 1 in/min (25 mm/min) based on ASTM FM VSS 302. Multi-Flex TPE contains Kratonâ„¢ G.Data provided by Multibase.
Physical Properties Metric English Comments
Density 1.16 - 1.22 g/cc
0.0419 - 0.0441 lb/in³
ASTM D792
Linear Mold Shrinkage 0.013 cm/cm
0.013 in/in
ASTM D955
Melt Flow 37.5 g/10 min
37.5 g/10 min
(Condition L) ASTM D-1238
Mechanical Properties Metric English Comments
Hardness, Shore A 60
60
10 sec; ASTM D-2240
Tensile Strength, Ultimate >= 3.62 MPa
>= 525 psi
ASTM D412
Elongation at Break >= 500 %
>= 500 %
ASTM D412
Flexural Modulus 0.0345 GPa
5.00 ksi
method 1, Proc.B; ASTM D-790
Tear Strength >= 19.26 kN/m
>= 109.9 pli
ASTM D624