Material Notes:
Multi-Flex TPE contains Kraton™ G.Data provided by Multibase.
Physical Properties Metric English Comments
Density 0.982 g/cc
0.0355 lb/in³
ASTM D792
Linear Mold Shrinkage 0.015 cm/cm
0.015 in/in
ASTM D955
Melt Flow 8.7 g/10 min
8.7 g/10 min
(Condition L) ASTM D-1238
Mechanical Properties Metric English Comments
Hardness, Shore A 91
91
10 sec; ASTM D-2240
Tensile Strength, Ultimate 13.1 MPa
1900 psi
ASTM D412
Elongation at Break 613.1 %
613.1 %
ASTM D412
Flexural Modulus 0.173 GPa
25.1 ksi
method 1, Proc.B; ASTM D-790
Tear Strength 64.6 kN/m
369 pli
ASTM D624