Multibase SILASTIC® C7-4535 DICUP R Dow-Corning Biomedical Grade ETR Elastomer

Category Polymer , Thermoplastic , Elastomer, TPE , Silicone, Thermoplastic
Manufacturer Multibase
Trade Name SILASTIC®
Port Shanghai port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Multibase SILASTIC® C7-4535 DICUP R Dow-Corning Biomedical Grade ETR Elastomer.pdf
Price EMAIL US    sales@lookpolymers.com
Material Notes:
Information provided by Multibase
Mechanical Properties Metric English Comments
Hardness, Shore A 33
33
as molded
34
34
post cured- 2 hours at 177°C
39
39
post cured- 4 hours at 204°C
Tensile Strength, Ultimate 5.93 MPa
860 psi
post cured- 4 hours at 204°C
8.34 MPa
1210 psi
post cured- 2 hours at 177°C
8.446 MPa
1225 psi
as molded
Tensile Strength, Yield 1.07 MPa
155 psi
at 200%, as molded
1.24 MPa
180 psi
at 200%, post cured- 2 hours at 177°C
1.38 MPa
200 psi
200%, post cured- 4 hours at 204°C
Elongation at Break 683 %
683 %
post cured- 4 hours at 204°C
943 %
943 %
post cured- 2 hours at 177°C
977 %
977 %
as molded
Tear Strength 24.7 kN/m
141 pli
post cured- 2 hours at 177°C; Die B
27.0 kN/m
154 pli
post cured- 4 hours at 204°C; Die B
27.7 kN/m
158 pli
as molded; Die B