Nabaltec GRANALOX® NM 9922 I Ceramic Bodies

Category Ceramic , Oxide , Aluminum Oxide
Manufacturer Nabaltec GmbH
Trade Name GRANALOX®
Port Ningbo port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Nabaltec GRANALOX® NM 9922 I Ceramic Bodies.pdf
Price EMAIL US    sales@lookpolymers.com
Material Notes:
Nabaltec`s GRANALOX® Ceramic bodies are produced under rigid quality control of green and sintered density, shrinkage, porosity, loss on ignition and granulate size. The properties of the corundum are tailored to the application areas in which the material is used such as wear resistance, high temperature stability, good electrical insulation, thermal conductivity and corrosion resistance.Used in engineering ceramics.
Physical Properties Metric English Comments
Bulk Density 1.00 - 1.10 g/cc
0.0361 - 0.0397 lb/in³
Density 3.88 - 3.92 g/cc
0.140 - 0.142 lb/in³
Sintered Density
Moisture Absorption at Equilibrium 0.10 - 0.30 %
0.10 - 0.30 %
Loss On Ignition 4.5 %
4.5 %
Particle Size 50 - 80 µm
50 - 80 µm
Median Grain Diameter
Thermal Properties Metric English Comments
Shrinkage 17 - 18 %
17 - 18 %
linear
Component Elements Properties Metric English Comments
Al2O3 99.7 %
99.7 %
Na2O 0.10 %
0.10 %
Processing Properties Metric English Comments
Sintering Temperature 1600 °C
2910 °F
1550 - 1700 °C
2820 - 3090 °F
Interval (dense ceramic parts)
Descriptive Properties Value Comments
Dwell Time hr. 2