Material Notes:
Description: Softflex® Thermoplastic Elastomer AlloyInformation provided by Network Polymers Inc.
Physical Properties Metric English Comments
Specific Gravity 0.910 g/cc
0.910 g/cc
ASTM D792
Linear Mold Shrinkage, Flow 0.017 cm/cm

@Thickness 3.17 mm
0.017 in/in

@Thickness 0.125 in
ASTM D955
Linear Mold Shrinkage, Transverse 0.015 cm/cm

@Thickness 3.17 mm
0.015 in/in

@Thickness 0.125 in
ASTM D955
Melt Flow 45.5 g/10 min

@Load 1.00 kg,
Temperature 235 °C
45.5 g/10 min

@Load 2.20 lb,
Temperature 455 °F
Procedure A Condition Q; ASTM D1238
Mechanical Properties Metric English Comments
Hardness, Shore A 30 - 40
30 - 40
10 second dwell; ASTM D2240
34 - 44
34 - 44
Instantaneous; ASTM D2240
Tensile Strength, Yield 4.00 MPa
580 psi
chs 20 in/min; ASTM D412
Elongation at Break 950 %
950 %
ASTM D412
Gardner Impact >= 36.2 J

@Temperature -30.0 °C
>= 26.7 ft-lb

@Temperature -22.0 °F
ASTM D5420
Tear Strength 22.8 kN/m
130 pli
ASTM D624