Material Notes:
Good oil resistance with good compression set properties, great for extruded artifacts with good mechanical properties.Applications: rolls, printing rolls, hose tubes and cover stocks, profiles, calendared sheet for die cut gaskets, coated fabrics and mould goods.Information provided by Dax Resinas
Physical Properties Metric English Comments
Volatiles 0.00 - 0.70 %
0.00 - 0.70 %
Method B-003; ASTM D5668
Mooney Viscosity 75 - 85

@Temperature 100 °C
75 - 85

@Temperature 212 °F
ML1+4, Method B-002; ASTM D1646
Ash 0.00 - 1.0 %
0.00 - 1.0 %
Method B-007; ASTM D5667
Descriptive Properties Value Comments
Appearance Light beige to yellowish
Bound Acrylonitrile Content (%) 31 - 34
ASTM D3533
Mh (lbf.in) 27.0-40.0
ASTM D2084
ML (lbf.in) 8.0-15.0
ASTM D2084
Polymerization Cold
Tsl (min) 2.0-4.5
ASTM D2084