| Category | Ceramic , Oxide , Silicon Oxide , Other Engineering Material , Additive/Filler for Polymer |
| Manufacturer | Nyco |
| Trade Name | ULTRAFIBRE® |
| Port | Shanghai port,China |
| Trade Terms | EXW, FOB, CFR, CIF |
| Payment Terms | L/C, T/T, PayPal |
| Download PDF | Nyco ULTRAFIBRE® 30 Wollastonite.pdf |
| Price | EMAIL US sales@lookpolymers.com |
| Physical Properties | Metric | English | Comments |
|---|---|---|---|
| Bulk Density | 0.400 g/cc | 0.0145 lb/in³ | Loose |
| 0.800 g/cc | 0.0289 lb/in³ | Tapped | |
| Density | 2.90 g/cc | 0.105 lb/in³ | |
| Brightness | 82 % | 82 % | G.E. Brightness |
| Oil Absorption | 35 % | 35 % | |
| Solubility in Water | 0.0095 % | 0.0095 % | |
| Moisture Absorption | 0.0200 % | 0.0200 % | |
| Particle Size | >= 15 µm | >= 15 µm | 10% smaller than |
| 55 µm | 55 µm | median; Microtrac | |
| <= 200 µm | <= 200 µm | 90% smaller than | |
| pH | 9.9 | 9.9 | 10% Slurry |
| Specific Surface Area | 0.40 m²/g | 0.40 m²/g | BET |
| Molecular Weight | 116 g/mol | 116 g/mol |
| Mechanical Properties | Metric | English | Comments |
|---|---|---|---|
| Hardness, Mohs | 4.5 | 4.5 | |
| Tensile Strength | 2700 - 4100 MPa <br>@Diameter 0.00300 - 0.150 mm |
392000 - 595000 psi <br>@Diameter 0.000118 - 0.00591 in |
Fiber Strength |
| Modulus of Elasticity | 303 - 530 GPa <br>@Diameter 0.00300 - 0.150 mm |
43900 - 76900 ksi <br>@Diameter 0.000118 - 0.00591 in |
Fiber Modulus |
| Thermal Properties | Metric | English | Comments |
|---|---|---|---|
| CTE, linear | 6.50 µm/m-°C | 3.61 µin/in-°F | |
| Thermal Conductivity | 2.63 - 2.77 W/m-K | 18.3 - 19.2 BTU-in/hr-ft²-°F | |
| Melting Point | 1410 °C | 2570 °F | ASTM D1857 |
| 1540 °C | 2800 °F | theoretical |
| Optical Properties | Metric | English | Comments |
|---|---|---|---|
| Refractive Index | 1.63 | 1.63 |
| Component Elements Properties | Metric | English | Comments |
|---|---|---|---|
| Al2O3 | 0.40 % | 0.40 % | |
| CaO | 46.36 % | 46.36 % | |
| Fe2O3 | 0.77 % | 0.77 % | |
| K2O | 0.020 % | 0.020 % | |
| Loss on Ignition(%) | 0.50 % | 0.50 % | |
| MgO | 0.15 % | 0.15 % | |
| MnO | 0.15 % | 0.15 % | |
| SiO2 | 51.6 % | 51.6 % | |
| TiO2 | 0.050 % | 0.050 % |
| Electrical Properties | Metric | English | Comments |
|---|---|---|---|
| Electrical Resistivity | 1.30e+13 ohm-cm | 1.30e+13 ohm-cm | pure wollastonite |
| Dielectric Constant | 6.8 <br>@Frequency 10000 Hz |
6.8 <br>@Frequency 10000 Hz |
|
| 6.8 <br>@Frequency 100000 Hz |
6.8 <br>@Frequency 100000 Hz |
||
| 6.9 <br>@Frequency 1.00e+6 Hz |
6.9 <br>@Frequency 1.00e+6 Hz |
||
| 6.9 <br>@Frequency 1000 Hz |
6.9 <br>@Frequency 1000 Hz |
||
| Dissipation Factor | 0.00152 <br>@Frequency 1000 Hz |
0.00152 <br>@Frequency 1000 Hz |
|
| 0.0046 <br>@Frequency 10000 Hz |
0.0046 <br>@Frequency 10000 Hz |
||
| 0.0046 <br>@Frequency 1.00e+6 Hz |
0.0046 <br>@Frequency 1.00e+6 Hz |
||
| 0.0078 <br>@Frequency 100000 Hz |
0.0078 <br>@Frequency 100000 Hz |
| Descriptive Properties | Value | Comments |
|---|---|---|
| Appearance | White | |
| Bulking Value (gal./lbs.) | 0.0413 | |
| Minus 100 U.S. Mesh Screen (%) | 99 | |
| Morphology | Acicular | |
| Sedimentation (cm) | 42 |